Relieving Stress in Box Construction Welds
Hey all, I'm working on a square steel tubing frame here at work, and I'm running into some difficulties with keeping everything nice and square. No matter how I seem to clamp, tack, and patch weld the corners of the tubing to each other, they always seem to end up "snapping" out of square when I release the clamps. I was wondering if there is a reasonably simple way to relieve the stress in the welds to keep everything nice and square, or any tips you could give me on my welding technique to keep this from happening in the first place. I'm running a Millermatic 211 MIG machine with .035 solid wire at 230v, wire speed set to 50, voltage set to 14 gauge. The material is 14 gauge 1.5"x1.5" tubing.
Posted Jun 16, 2015, 3:50 PM UTC
518