Entry level pre employment.
Hi , I just want to ask some few question. I have been going to school to get my certificate for 2 months. I just finished yesterday and got an offer at Ingalls shipyard to take the pre employment welding. It’s 3G stick and Mig. A few question is... I haven’t been taught on how long to wait after root and hot pass. How long does the plate normally sits to cool down? Any tips and tricks?! I do my stick at 100 amps and I do passes and caps perfect and was told do it at 113.. what’s the logic behind that? Or just stick on what I know?! I appreciate any feedback! Thank you!!
Posted Sep 22, 2018, 7:38 PM UTC
The amp thing probably has to do with their inhouse WPS. And for the plates, my welding teachers told me to place my hand above the plate without gloves on. When it feels like you could touch it (don't) it should be ok to do the next bead.
Thank you so much this is a very good tip!!! Would do this for my practice on Monday!!
Then again the minimum interpass temperature for some tines I do at work is 600 degrees. It has a lot to do with material thickness and I imagine that a shipyard would have you running hot as possible.
Most of our shipyards WPS state 300 degrees celsius as max temp. But I guess it depends on what you work with. That is mainly A36-E36 steel.
It certainly does. This is for AR steel on forklift tines.