What most likely caused the oxidisation of the veroboard here? Can I do something to avoid it in future?

Posted Jul 1, 2021, 9:31 AM UTC

Posted Jul 1, 2021, 9:31 AM UTC
Given that the spot in question is on the substrate rather than copper, I don't think oxidation is to blame. Some alternative theories:
The flux was not completely cleaned off this spot after soldering, and dust / dirt stuck to it.
The flux was not completely cleaned off this spot after soldering, and it has become conductive.
You mentioned that this is a power rail. Some exterior, conductive object may be making intermittent shorts across the joints, and this is causing the top layer of substrate to burn.
An over-voltage condition is causing arcing across the joints, and this is causing the top layer of substrate to burn.
Try to clean the spot with some isopropyl alcohol. If it easily comes off, it was probably flux. If not, it might be burnt substrate. In the latter case, you need to get in there and dig out every last bit of black stuff that you see. It is conductive, and will worsen over time if you leave it there.
Thanks - it was hard to take a good photo with my phone but I looked at it under the microscope and it was indeed some residue on top of the board rather than the board itself. I think it must have been flux. It was easy to scrape off using fine tweezers.
So my takeaways are, clean and polish with steel wool before soldering, clean much more thoroughly afterwards, apply coating when it's tested and working, and put it in a box or bag for the long term.
Thanks to all for the advice!
For stuff that isn't mission critical, I usually skip most of that and just clean the flux after soldering. Depends on the application, of course.
Sure - if it was mission critical I'd make a proper PCB anyway - I'm still interested in learnng what the best practices are though, and what the consequences are of not following them, so this is all good!
This looks like either flux scum from repeated soldering, or an arcing problem....
I don't know if it's just the shadows, but indeed looks like it could be some form of arcing, and OP said it's between GND and 5V so that would make sense.
keep the board in air tight box. avoid it to moisture contact
Also to put silica gel packets or the reusable ones
Thanks - I nearly did, but didn't quite get around to it, and ended up just using it out in the open. I'll do that in future!
A product I use to keep breadboards made of double side PCB material clean and bright after assembly is a product such as Krylon clear acrylic coat or similar aerosol acrylic coating. I have 15 year old breadboards and the copper remains as bright as the day I polished the copper with an abrasive pad.
Great, thanks - I guess you polish it before soldering to get better joints? I found this much harder to solder than a PCB, in spite of cleaning it with IPA beforehand - at the time I thought it was just the lack of solder resist and the heat capacity of the traces that was making it difficult.
The copper like any other metal will tarnish or form a layer which is difficult for rein to break through. That is why I polish the board before soldering. Then I wash the board in 195 proof ethanol if it is a keeper, dry it and then spray with Krylon. Krylon does extremely well indoors and it is fair outside. The trick is to start with clean bright copper, then clean the flux off and then overspray with Krylon a couple of times. If you need to solder soemthing later the Krylon vaporizes. Once done with the mod or repair overspray it again.
Air does that. If you need to solder it, best thing is a extra fine steel wool ball (like the ones used for pots) . Just very lightly wipe the board and you will e good.
Make sure you don't get high on the fumes!
Alternatively you could tin the Veroboard. What we did at high school.
I kind of did that by accident in some places!
Oxidation? Probably oxygen 😬
I always use one of these "PCB Eraser" before starting to assemble and solder a project: https://kitronik.co.uk/products/2662-pcb-eraser
I just hit the copper with a Scotch-Brite pad
This is between ground and a 5V power rail (after a P-MOSFET), on veroboard, and there's no sign of similar oxidisation elsewhere where they also run parallel to each other, including where the power enters the board which is also two solder joints right next to each other. It developed over a period of several months.
I doubt I've got any liquid to that specific point, but it is between two solder joints. Could it be excess heat during soldering, or flux splashes?
Mostly I'd like to know what I could do differently to avoid this in future, thanks for any help!
[removed]
Air, particularly the moisture in it.
Keep in a sealed bag with desiccant sachet before use. Ensure to use a good flux to ensure any oxidation is cleared under the solder joint.
Coat with conformal coat / PCB lacquer after soldering: https://www.techspray.com/the-essential-guide-to-conformal-coating
Great, thanks, I'll check it out! I have been using it in the open air, with no coating applied, so that all lines up. I'll also take more care to clean the flux off afterwards on future boards, as I can still see it bridging between the tracks.