OldLabRat

u/OldLabRat


r/Teachers•

If you have ever moved a chemistry classroom to a new school building, please take a minute to inform me on which chemicals you were able to pack for moving, and which ones needed to be disposed of. I am under an urgent deadline, needing to come up with the 2026-2027 budget by the end of this week, so any information that you can provide would be appreciated.

I thank you in advance for any information you can give me.

12

r/Teachers•

Can anyone point me to a good resource that will help me understand how this is done in ASPEN? I would like to understand the process of building a master schedule. Videos, books, anything that could help? I am actually pretty good at math, and this seems like a math problem involving constrained optimization, but I do want to get up to speed on the process before I make any suggestions.

Also, I have never served on a committee of this sort. How are advisory committees managed at your school. Are they a committee of faculty alone? Or are they led by an administrator? I can imagine two possible extremes: in one extreme, I imagine a democratic committee of faculty alone who vote on

02



r/chemistry•

Copper (I) oxide is commonly called 'red copper oxide' but I have yet to make anything that looks really 'red' to me. Does anyone have any ideas for making Cu₂O for pigment applications, and does it really get 'red'?

My current method is to prepare a solution of CuSO₄ and trisodium citrate. Following this, I add a solution of glucose as a reducing agent. I bring the solution to a near-boil and slowly add NaOH solution: this causes Cu₂O to precipitate, first as a yellowish material, then a more vibrant orange-red, and if I continue adding NaOH it soon starts to turn darker/brownish. I have read that this has something to do with nanoscale properties of the precipitate, but I'm not sure

25


r/chemistry•

​

2:1 Calcium Chloride/Water Mix

Dollar tree aluminum bowl with 200 g CaCl2 and 100 g H2O. Got it up to 170 C before the boiling got too vigorous to deal with. Nice crust of solid CaCl2 on top keeps it from evaporating too fast, I think. Might be able to push it hotter but it's definitely enough for refluxing an esterification or something. And it looks cool. It's pretty much completely solid below 100 C so it won't spill easily.

[Sand bucket next to CaCl2 bath](https://preview.redd.it/hriepulcd1ka1.jpg?width=1791&forma

16