Been printing some larger pieces and containers with larger wall sections 1-5mm thick, >20cm wide/high out of HIPS/.. recently. Have been doing it with a Bambu A1 in a "tent" and a heater that brings the air temp up to around 45C. Printbed adhesion is there with glue.
Big issue I face is that these pieces tend to show stress cracking in all directions either during chemical smoothing with eg acetone for HIPS, or being exposed to heat to around 70C.
Is it possible to temper these printed pieces somehow to release/even out stress without loosing shape by heating to the materials Tc followed by a soak and slow cooldown? In an regulated oven for example. Would be happy about feedback from prac